Tbm High Performance Steel Cord Conveyor Belting
Yiwu Yaosheng Daily Products Co., Ltd. / 2022-06-27
- Type:Steel Cord Conveyor Belt
- Material:Rubber
- Inside Material:Steel Cord
- Feature:Oil-Resistant, Acid And Alkali Resistant, Tear-Resistant, Heat-Resistant, Cold-Resistant, Wear-Resistant
- Tensile Strength:Strong
- Transport Package:Standard Packing
=== Base Info ===
- Model NO.:ST Series
- Specification:GB, DIN, RMA, ISO, AS, SABS, BS
- Trademark:JIUZHOU
- Origin:Baoding City, Hebei, China
- HS Code:40101100
- Production Capacity:2000 Meters Per Day
=== Description ===
Cord Number
500 ±5 | 39 | 34 | | | | | | | | | |
650 ±7 | 51 | 44 | | | | | | | | | |
800 ±8 | 64 | 55 | 50 | 64 | | | | | | | |
1000 ±10 | 81 | 69 | 64 | 81 | 64 | 64 | 64 | 64 | 59 | 55 | 55 |
1200 ±10 | 97 | 84 | 77 | 97 | 77 | 77 | 77 | 77 | 71 | 66 | 66 |
1400 ±12 | 114 | 98 | 90 | 114 | 90 | 90 | 90 | 90 | 84 | 78 | 78 |
1600 ±12 | 131 | 112 | 104 | 131 | 104 | 104 | 104 | 104 | 96 | 90 | 90 |
1800 ±14 | 147 | 127 | 117 | 147 | 117 | 117 | 117 | 117 | 109 | 102 | 102 |
2000 ±14 | 164 | 141 | 130 | 164 | 130 | 130 | 130 | 130 | 121 | 113 | 113 |
2200 ±15 | 181 | 155 | 144 | 181 | 144 | 144 | 144 | 144 | 134 | 125 | 125 |
2400 ±15 | 197 | 169 | 157 | 197 | 157 | 157 | 157 | 157 | 146 | 137 | 137 |
2600 ±15 | 214 | 184 | 170 | 214 | 170 | 170 | 170 | 170 | 159 | 149 | 149 |
2800 ±15 | 231 | 198 | 170 | 214 | 170 | 170 | 170 | 170 | 159 | 149 | 149 |
3000 ±15 | 247 | 212 | 197 | 247 | 197 | 197 | 197 | 197 | 184 | 172 | 172 |
3200 ±15 | 264 | 227 | 210 | 264 | 210 | 210 | 210 | 210 | 196 | 184 | 184 |
Mining Conveyor Belt | Lump Size | Temperatrure of Materials Carried | Belt Surface Temperature |
Coke | 100~200mm(4~8 inch) | 70~100 ºC | 50~60 ºC |
Cement | Powder | 100~250 ºC | 80~90 ºC |
Clinker | 10~30 mm (0.4~1.2 inch) | 100~220 ºC | 100~110 ºC |
Molding | -- | 200~250 ºC | 80~90 ºC |
Metal Powder | -- | 170 ºC | 120~130 ºC |
Raw Material | below 30mm(1.2 inch) | 180~220 ºC | 100~120 ºC |
Sintered Ore | 25~200 mm(1~8i nch) | 200~400 ºC | 130~150 ºC |
Return of Sintered Ore | below 10mm(0.4 inch) | 260 ºC | 180~200 ºC |